Spray Stone surface prep and troubleshooting
Spray Stone covers a lot, but not cracks, damp or loose render. Here’s how to read and prepare a wall, the conditions to work in, and how to fix the most common problems.
Sound, clean and dry: the base of every stone finish.
Spray Stone covers a lot, but it won’t hide cracks, damp or loose render. Here’s how to inspect and prepare a wall, the weather to work in, and how to fix the problems that show up most.
- +5 °Cminimum air and wall temperature
- +10 to +25 °Crecommended range for exterior walls
- 1–4 htypical dry time for primer and Hydro Paint
- 0active cracks you should ever coat over

Is today a good day to spray?
Air and wall temperature both count. Set the temperature to check, and tick the box if it’s damp or rain is due.
Recommended +10 °C to +25 °C for the air and the wall, and never below +5 °C. Avoid rain, frost, fog, strong wind, hot surfaces and direct sun.
Recommended +10 °C to +25 °C for the air and the wall, and never below +5 °C. Avoid rain, frost, fog, strong wind, hot surfaces and direct sun.
Wind
Don’t spray in wind that stops you controlling the pattern. It wastes material and spreads overspray.
Dew point
Check air and wall temperature, humidity, dew point and the overnight forecast before you start.
Sun
Work on shaded elevations where you can, and avoid excessively hot surfaces.
Read the wall before you coat it.
Pick what you’ve found. Each tab says what to do before the primer goes on.
Class every crack: hairline, stable, shrinkage, localised, recurring, movement-related or structural. Never coat over active cracking; find and correct the cause of the movement first.
Repairing stable cracks
Open the crack enough to repair it, remove loose material and dust, fill it with a compatible exterior-grade material and finish it level with the wall. Let repairs cure and dry before priming.
Movement joints
Keep designed movement and expansion joints working. Don’t bridge them rigidly.
Remove loose or poorly bonded render, paint, old coatings and repairs. Repair holes, missing render, impact damage, deep defects and failed repairs.
Spray Stone isn’t a levelling compound. Correct significant imperfections before you start, so the texture sits on a sound, even wall.
Remove efflorescence, moss, algae and other growth, and let the wall dry. Don’t coat a wall with active water ingress or significant damp.
Fix the source first: leaking gutters, failed flashings or a defective roof. The PU Topcoat protects the finish; it won’t waterproof defective construction.
New render and cement-based materials need to be properly cured before coating. The wall must be sufficiently dry, not holding active moisture, stable and secure.
Clean off construction residue and dust, then prime with Infinity alkali-resistant wall primer.


Tick these off before you prime.
Something’s not right? Find the fix.
Filter by type, then tap a problem for the likely cause and what to do.
!Sagging, runs or slow dryingConditions
Low temperatures, or too much material in one pass.
Stop and let it dry. Carry on only inside the temperature range, building texture with lighter passes.
Check the forecast and wall temperature before you start.
!Lap marks or dry sprayConditions
Strong direct sun or hot surfaces.
Move to shaded elevations and keep a consistent, wet pattern.
Plan the day around the sun.
!Overspray and a ragged patternConditions
Wind.
Stop spraying until you can control the pattern again.
Check the wind first, and screen the work area if you can.
!Patchy texture or heavy spotsApplication
Changes in spray distance or air pressure, or too much build in one go.
Go back to the sample panel and keep settings steady.
Build texture through controlled passes.
!Texture differs between areasApplication
Different settings or technique between operators.
Work to one approved sample, with equivalent settings for everyone.
Agree the sample before anyone starts spraying.
!Visible joins mid-wallApplication
Stopping partway across a large, uninterrupted wall.
Talk to our technical team about the best way to blend it.
Only stop at natural breaks: corners, joints, downpipes and features.
!Recesses missed by the topcoatTopcoat
Incomplete PU Topcoat coverage over the texture.
Apply controlled, overlapping passes that reach recesses, corners and reveals.
Spraying the topcoat helps on textured stone.
!Poor adhesionAdhesion
An unsuitable surface, contamination, or a layer that wasn’t dry.
Remove the loose material, re-prepare and let every layer dry before the next.
Use Infinity primer and Hydro Paint. Other products can affect adhesion and breathability.
!Cracks coming back throughSubstrate
Active or structural movement in the wall behind.
Find and correct the cause of the movement before recoating.
Never use Spray Stone to hide or bridge structural or moving cracks.
From tired walls to stone.
Before-and-afters and finished walls from our fitters.
More in the Spray Stone guide series
Questions we get asked
Can Spray Stone cover cracks in render?
Not active or structural ones. Find and correct the cause of any movement first. Stable cracks can be opened, repaired with a compatible exterior-grade material and left to cure before you prime.
What’s the lowest temperature I can spray at?
Never below +5 °C, for the air and the wall. The recommended range for exterior walls is +10 to +25 °C.
Can I spray in direct sun?
Avoid it. Hot surfaces in strong sun cause lap marks, dry spray and uneven drying, so work on shaded elevations where you can.
Does Spray Stone level an uneven wall?
No. It isn’t a levelling compound, so correct significant imperfections before you start.
Can I use another primer?
Use Infinity primer and Hydro Paint. Unapproved primers, paints or topcoats can affect adhesion, breathability and appearance.
Keep reading
All news & guides
One factory, every surface: which Infinity system?Which Infinity system for your project? Pick the surface, from worktops and kitchen doors to floors, walls, driveways, uPVC and furniture, and see the system.26 Nov 2026 · 4 min readRead the guide
Start a coatings business with InfinityHow to start a coatings business with Infinity Effects: pick your services, train and certify, open a trade account, get found and grow.26 Nov 2026 · 3 min readRead the guide
How to order from Infinity EffectsHow to order from Infinity Effects: set up your account, build your kit list, check out and choose delivery, with dispatch times and where we ship.26 Nov 2026 · 3 min readRead the guide