Explore the Possibilities. Together.

Guides & how-toInfi-Rox Binder

Infi-Rox base prep and troubleshooting

Most resin bound problems start in the base. Here’s how to check and prepare concrete, tarmac, a new SuDS base, internal floors and walls, when to lay, and how to fix the problems that show up most.

RMRyan McGovernLead chemist & formulator, Infinity Effects26 Nov 2026 · 6 min read
Infi-Rox Binder · Resin

A resin bound surface is only as good as the base under it.

Infi-Rox goes over sound concrete or tarmac, onto a new permeable SuDS base, indoors as a stone carpet, or up a wall. Here’s how to check and prepare each base, the weather to lay in, and how to fix the problems that show up most.

  • < 6%moisture in concrete before priming
  • 25 MPa+recommended concrete strength
  • 1:60–1:80falls on a new SuDS base
  • 10–25 °Cideal laying range
Primer being rolled over the mesh before the stone goes down, by Costa Resin & Construction
Costa Resin & Construction · Primer and mesh stageSee the job →
Before you start

Is today a good day to lay?

Set the temperature to check, and tick the box if the base is damp or rain is forecast.

Lay between 5 °C and 30 °C, ideally 10–25 °C. Avoid direct sun, high winds, frost and rain, and don’t start if rain is forecast.

Check the conditions

Lay between 5 °C and 30 °C, ideally 10–25 °C. Avoid direct sun, high winds, frost and rain, and don’t start if rain is forecast.

1

Dew point

Monitor temperature, humidity and dew point through the job.

2

Dry, stable materials

Keep resin and stone at a stable temperature, and the stone completely kiln-dried.

3

Shelter

A mixing tent and a forced-air heater help on cold or changeable days.

Prep by base

Getting the base ready to prime.

Pick what you’re laying on.

Check it

Clean, dry, structurally sound and free from contamination, with moisture below 6% and pH below 10. 25 MPa or more is recommended. Never lay onto damp or green concrete.

Repair it

Look for cracks, spalled or loose material, depressions, movement joints and weak or powdery concrete. Fill cracks with repair mortar and grind high spots.

Open it up

Mechanically abrade or diamond-grind where needed for a clean, open profile, then vacuum. Mask walls, edging, drain covers and doors.

A resin bound job in progress in Wicklow, by Premres
Premres · Job in progress · July 2026See the job →
Power-trowelling a resin bound driveway, by Costa Resin & Construction
Costa Resin & Construction · Driveway, power trowel · November 2026See the job →
Ready check

Tick these off before you prime.

0/7

Work through the list

Most resin bound problems start in the base.

Open the install guide
Troubleshooting

Something’s not right? Find the fix.

Filter by type, then tap a problem for the likely cause and what to do.

!Loose stonesMixing
Likely cause

Not enough binder, poor mixing, or poor compaction.

Fix it

Keep to the binder quantities, mix until every stone is coated, and compact thoroughly.

Next time

Use accurate weights and a forced-action mixer.

!Patchy appearanceMixing
Likely cause

Uneven mixing or application, or variation in the stone.

Fix it

Use accurate weights, consistent mixing times and consistent trowelling.

Next time

Keep every batch the same, start to finish.

!Whitening or hazeWeather
Likely cause

Moisture during the cure, or low temperatures.

Fix it

Protect the surface from rain and dew while it cures.

Next time

Never start if rain is forecast, and never lay on a damp base.

!CrackingBase
Likely cause

Movement in the base, not enough mesh, or poor installation.

Fix it

Find and fix the movement before any repair.

Next time

Use CRM Mesh where specified, with full overlaps.

!Sticky surfaceCure
Likely cause

The wrong mix ratio, low temperature, or too short a cure.

Fix it

Give it longer to cure; if it stays tacky, ask our technical team.

Next time

Use complete kits, and lay inside the temperature range.

!Rough trowel finishTrowelling
Likely cause

Overworking the surface.

Fix it

Use light, controlled strokes and correct the surface while it’s still workable.

Next time

Keep trowels clean with Safe Solvent or ROX Trowel Cleaner.

!Slow drainage on a SuDS baseSuDS
Likely cause

An over-trowelled base course.

Fix it

Ask our technical team before going further.

Next time

Compact the base course without over-trowelling it.

!Stone sliding off a wallVertical
Likely cause

Not enough tack, too thick a lift, or the wrong stone.

Fix it

Allow more tack, reduce the thickness and check the stone size.

Next time

Wait until the tack coat is tacky and the mix clumps.

!Shutter stickingVertical
Likely cause

Resin bonded to untreated timber or MDF.

Fix it

Use release tape or a non-stick facing.

Next time

Tape every timber face that touches the resin.

Real jobs

Laid on a proper base.

Infi-Rox jobs from our installers.

FAQ

Questions we get asked

How dry does concrete need to be?

Below 6% moisture, with pH below 10. Never lay onto damp or green concrete.

What falls does a SuDS base need?

Falls of 1:60 to 1:80, checked at the sub-base and capping layers.

How deep is the Type 3 sub-base?

125 mm as standard, increased up to 225 mm where sub-soil permeability is a concern, compacted in 75–100 mm layers.

Can I lay in the rain?

No. Don’t start if rain is forecast, and never lay in rain, on standing water or in freezing conditions.

What causes loose stones?

Not enough binder, poor mixing or poor compaction. Keep to the binder quantities and mix until every stone is coated.

Downloads & tools
Having it done?Find an Infinity-trained installer near youFind an installerInstalling it yourself?Learn the system at an Infinity Effects certified schoolSee the training

Keep reading

All news & guides

Leave a Comment

Your email address will not be published. Required fields are marked *