R.S.P pour surface prep and troubleshooting
Most pour failures start before the resin is mixed. Here’s how to get worktops and concrete floors ready, how temperature changes your working time, and how to fix the problems that come up most.
Sound, clean, dry, abraded: the pour is only as good as the prep.
Most pour failures start before the resin is mixed: a skipped primer, a missed tack window or a contaminated surface. Here’s how to get worktops and floors ready, how temperature changes the clock, and how to fix what goes wrong.
- CSP 2–3profile for concrete floors
- 220–400grit to abrade worktops
- −10 °CR.S.P goes down to this without heaters
- MandatoryR.S.P Primer, in every system

How will today’s temperature change the pour?
Cold isn’t a problem for R.S.P, but temperature changes how long you have. Set the temperature to check.
R.S.P can be applied down to −10 °C without heaters. Fast Set’s 20-minute gel time is measured at 15 °C: warmth shortens it, and cold slows the cure.
R.S.P can be applied down to −10 °C without heaters. Fast Set’s 20-minute gel time is measured at 15 °C: warmth shortens it, and cold slows the cure.
Organise first
Prime, tape and lay out colours and tools before you mix. Lost working time is usually lost to set-up.
Small batches
Mixed resin warms itself as it reacts. Mix only what you can pour, and get it out of the bucket.
Dust-free air
Keep the area clean, dry and free from airborne dust, with good ventilation while you work.
Getting the surface ready to prime.
Pick what you’re pouring onto.
Clear and clean
Take out appliances and fittings for full access. Remove grease, silicone, wax, oils and cleaning residue, and protect the cabinets, walls, splashbacks and flooring around the top.
Abrade
Sand the whole top with 220–400 grit to remove the gloss and give a consistent key. Vacuum thoroughly, then go over it with a tack cloth: no sanding residue should remain.
Degrease
Wipe down with Fusion Degreaser / Adhesion Promoter, acetone or denatured alcohol, and let it dry completely. Fusion also chemically prepares difficult, low surface-energy surfaces.
Profile
Mechanically prepare the concrete to a CSP 2–3 profile. Deal with any unsound, dirty, greasy, contaminated or damaged areas first.
Edges
Prepare perimeters, edges and details properly, with no smooth areas left around the edge.
Vacuum
Vacuum thoroughly, especially edges, corners and joints. No loose dust should be left under the primer.
Can’t grind it?
Uneven floors, or floors you can’t grind, get a P.HB Screed base first (Floor System 1).
PolyFuse MAX is a fast-curing, high-strength polyaspartic repair filler for fine cracks, damaged concrete, broken expansion joints and edges.
Fine cracks
Use it neat, mixed 4:1.
Bigger repairs
Bulk it out with clean, completely dry sand to make a stronger repair mortar for larger cracks and deeper repairs.
It’s sandable and paintable, so sand repairs flush before you prime.
Drop a little water on the surface. If it soaks in and darkens it, the surface is porous.
Porous surfaces drink the primer, so give them a second coat of R.S.P Primer before you pour. Build Your Pour adds it to your kit list when you tick porous.


Tick these off before you mix.
Something’s not right? Find the fix.
Filter by type, then tap a problem for the likely cause and what to do.
!Poor adhesion or delaminationAdhesion
Poor preparation, contamination or dust, no primer, or the base coat poured after the primer passed its tack stage.
Remove the affected material, re-prepare (CSP 2–3 on floors, 220–400 grit on worktops), prime again and pour while the primer is tacky.
Never skip R.S.P Primer, and pour inside its tack window.
!Fisheyes, or the resin pulling awayContamination
Oil, grease, silicone or other contamination on the surface.
Remove the source of the contamination, re-prepare and recoat.
Degrease properly before priming, and keep the area clean.
!Dust or debris in the finishContamination
Dust or debris landing during application or cure.
Keep the area controlled, and protect the surface while it cures.
Vacuum and tack-cloth before priming, and work in still, dust-free air.
!Uneven pour depthApplication
Poor levelling or distribution.
Use the correct notched squeegee and a levelling roller to keep an even build.
Level each area as you pour it.
!Thin or missed edgesApplication
Rushing perimeters, transitions and details.
Keep control at edges and detailed areas as you move the design.
Prepare edges properly, with no smooth areas left.
!Resin gelling before you’ve finishedWorking time
Poor organisation, a warm room or surface, or a full bucket left standing.
Prepare everything before mixing, mix only what you can pour, and add up to 5% Poly Extender where permitted.
Choose Slow Set, with its 2-hour gel time, for pours with design work.
!Patchy or uneven sheenTopcoat
Uneven topcoat application.
Spread the topcoat evenly and check under good light before it passes its workable stage.
Inspect under suitable lighting as you go.
Prepared properly, poured beautifully.
Pours from our fitters, on worktops and floors.
More in the R.S.P Polyaspartic guide series
Questions we get asked
What profile does a concrete floor need?
Mechanically prepare it to a CSP 2–3 profile, with no smooth areas left around the edges. Floors you can’t grind get a P.HB Screed base first.
How do I prepare a worktop for a pour?
Abrade the whole top with 220–400 grit, vacuum, go over it with a tack cloth, then degrease with Fusion Degreaser, acetone or denatured alcohol and let it dry completely.
Can I pour in the cold?
Yes. R.S.P can be applied down to −10 °C without heaters. It cures more slowly in the cold, so allow longer before use.
What causes fisheyes?
Contamination such as oil, grease or silicone. Remove the source, re-prepare and recoat.
How do I fill cracks before a pour?
Use PolyFuse MAX neat at 4:1 for fine cracks, or bulk it out with clean, completely dry sand for larger, deeper repairs. Sand it flush before priming.
Keep reading
All news & guides
One factory, every surface: which Infinity system?Which Infinity system for your project? Pick the surface, from worktops and kitchen doors to floors, walls, driveways, uPVC and furniture, and see the system.26 Nov 2026 · 4 min readRead the guide
Start a coatings business with InfinityHow to start a coatings business with Infinity Effects: pick your services, train and certify, open a trade account, get found and grow.26 Nov 2026 · 3 min readRead the guide
How to order from Infinity EffectsHow to order from Infinity Effects: set up your account, build your kit list, check out and choose delivery, with dispatch times and where we ship.26 Nov 2026 · 3 min readRead the guide